Poxycon

2C EPOXY WEAR LAYER AND REPAIR FOR FLOORS AND SCREEDS

Pressure-, wear- and weather-resistant.

Exceeds the cohesion of concrete.

Mechanical and chemical resistant.

poxycon-2kg-en-1024

Packaging

SKU EAN Description
poxycon-2kg-en 637219000 - 5415207000336 - Poxycon - pot 2kg 637219000 5415207000336 Poxycon - pot 2kg
poxycon-10kg-comp-ab-en 637220000 - - Poxycon - 10 kg 637220000 Poxycon - 10 kg

Description

Transparent, liquid 2-component epoxy resin for impregnating, reinforcing, priming, leveling, repairing, pouring, making encapsulation fluid-tight,…. Epoxy mortar is obtained by adding Poxy Quartz.

Technical information

poxycon-2kg-en-1024

Poxycon

2C EPOXY WEAR LAYER AND REPAIR FOR FLOORS AND SCREEDS

poxycon-2kg-en-1024
  • Density of the mixture at 25 ° C: 1.10 g / cm³.
  • Viscosity of the mixture at 25 ° C: 670 mPa.s.
  • Compression strength of 1:10 mortar:> 50 N / mm².
  • Flexural tensile strength of 1; 10 mortar:> 20 N / mm².
  • Pot life at 20°C and 60% R.V .: +/- 25min.
  • Processing temperature of material, substrate and environment: between + 8°C and + 30°C.
  • Humidity during processing: < 80%.
  • Drying times at 20 ° C and 60% RH: walkable after 1 day, mechanical load after 3 days and fully load after 7 days.
  • Chemical resistance after 7 days: resists acids, alkalis, oil, grease, gasoline, solvents and salt solutions, aggressive vapors, gases and sea air and most chemical products.
  • Shelf life: 12 months, keep dry, cool and frost-proof.
  • Safety measures: consult the Safety Data Sheet.

Instructions

Substrate

  • Apply to structurally strong, stable and clean substrate, free of loose particles, dust, oil, grease, rubber skid marks, etc.

Mixing

  • Remove the separation strip from the bag and then vigorously knead the two components in the bag for 1 minute to mix them.
  • Apply immediately.

Setting time

  • At 20°C and 60% RH, approx. 25 minutes.
  • At higher temperatures, the pot life is shorter, at lower temperatures it is longer.

Method

  • Depending on the project, use a rubber floor squeegee, a serrated rubber floor squeegee, a notched trowel, an epoxy roller, etc.

Waiting times

  • At +20°C, respect a waiting time of at least 12 hours and a maximum of 48 hours before applying a second coat.
  • If you expect the waiting time to be longer, the surface should be sprinkled with Poxy Quartz while the coat is still wet.
  • The curing time is shorter at higher temperatures and longer at lower temperatures.

Application temperature

  • Poxycon, ambient and substrate between +8°C and +30°C.

Curing time

  • At 20°C and 60% RH: can be walked on after 1 day, mechanically loaded after 3 days and fully loaded after 7 days.
  • This takes longer at lower temperatures.
  • Protect the Poxycon from moisture during the curing process (approx. 24 hours at +20°C) .

Some applications

  • Impregnate and/or strengthen Poxycon with a maximum of 20% Poxy DC, diluted on the surface until saturated.
  • Consumption will depend on the substrate and application: between 0.3 and 0.5 kg/m².

Primers

  • Apply Poxycon on the floor till it is saturated.
  • Consumption will depend on the substrate and application: between 0.3 and 0.5 kg/m².

Coloured wear layer

  • Pour half of the mixed Poxycon into the bucket.
  • Add 1 box of the selected Poxy Color and mix well until you obtain a homogeneous colour.
  • Add the rest from the bag and mix well.

Open-pore Poxycon mortar

  • Start by applying a base coat of Poxycon.
  • Then add the Poxy Quartz to the well-mixed Poxycon in the specially supplied bucket.
  • Mix thoroughly (3 minutes stirring time).
  • It is possible to use a slow-running mixer for that purpose.
  • Mixing ratio by weight: 1 part Poxycon and 10 parts Poxy Quartz.
  • Apply immediately.
  • Consumption per mm of coat thickness on 1 m²: approx. 0.2 kg of Poxycon and 2.0 kg of Poxy Quartz.

Liquid-tight Poxycon mortar

  • Start by applying a base coat of Poxycon.
  • Then add the Poxy Quartz to the well-mixed Poxycon in the specially supplied bucket.
  • Mix thoroughly (3 minutes stirring time).
  • It is possible to use a slow-running mixer for that purpose.
  • Mixing ratio by weight: 1 part Poxycon and 5 parts Poxy Quartz.
  • Apply immediately.
  • Consumption per mm of coat thickness on 1 m²: approx. 0.4 kg of Poxycon and 2.0 kg of Poxy Quartz.

Cleaning

  • Clean tools immediately after use and any fresh spills with Poxy DC.

Personal protective equipment

  • Suitable nitrile gloves, safety goggles and face protection.

Good to know:

  • Friction and mechanical load will wear the surface.
  • Stains may form during impregnation due to the difference in suction force.
  • Weather conditions and UV rays can affect colour stability negatively.
  • The base coat must offer sufficient pore filling. A second coat of Poxycon may therefore be required, or a thicker base coat.

Novatio minimises production downtime at Citrique Belge

See more
Poxycon_05

Order this item

A question?